What is ASTM SA612 (SA612M) steel plate steel grade?

Dec 17, 2025 Lăsaţi un mesaj

SA612 (SA612M) steel plate is a killed carbon–manganese–silicon (C–Mn–Si) steel designed for welded pressure vessel applications operating at moderate and lower temperatures.

 

The material is produced in accordance with ASME SA612/SA612M, ASTM A612/A612M, and is also manufactured under Wuyang Steel internal technical specification WYJ059-2006.

 

SA612 (SA612M) steel plate

 

SA612 steel plates are widely applied in petroleum, chemical processing, power generation, and nuclear-related industries, particularly for the fabrication of reactors, heat exchangers, spherical tanks, pressure vessels, and pressure-retaining shells.

 

 

SA612 steel plates are supplied in the normalized condition, which ensures uniform microstructure, improved toughness, and stable mechanical properties.

Standard thickness range (ASTM/ASME): <= 25 mm

Industrial production capability: 8 – 120 mm

Plate width: 1,500 – 4,100 mm

Plate length: 5,100 – 15,000 mm

 

Chemical Composition (wt.%)

 

The chemical composition of SA612 steel is strictly controlled to ensure strength, weldability, and low-temperature toughness.

C <= 0.25 <= 0.25
1.00 – 1.50 0.92 – 1.62
0.15 – 0.50 0.13 – 0.55
P <= 0.03 <= 0.03
S <= 0.02 <= 0.02
<= 0.35 <= 0.38
<= 0.25 <= 0.28
<= 0.25 <= 0.29
<= 0.08 <= 0.09
V <= 0.08 <= 0.09
<= 0.02* <= 0.03*
<= 0.03 <= 0.04
>= 0.020 >= 0.020

* Nb content may be increased to <= 0.05% (heat analysis) and <= 0.06% (product analysis) when required.

The controlled addition of Nb, V, and Ti promotes grain refinement and improves both strength and impact toughness.

 

 

Mechanical testing is conducted in accordance with SA612/SA612M requirements.

<= 12.5 mm 12.5 – 25 mm
570 – 725 560 – 695
>= 345 >= 345
Elongation (200 mm), % >= 16 >= 16
Elongation (50 mm), % >= 22 >= 22
Charpy V-notch Impact (–40℃, Transverse) Avg >= 27 J Single >= 20 J

Austenitic grain size: >= ASTM No. 5

Impact testing temperature: –40℃

These properties ensure reliable performance under internal pressure, thermal stress, and low-temperature conditions.

 

 

SA612 steel plates are manufactured under strict quality control systems:

Surface quality, edge condition, and weld repair: In compliance with SA-20M

Mill Test Certificates (MTC) are issued in accordance with SA-20M, including Al, Nb, and Ti content disclosure.

 

 

SA612 steel plates are extensively used in pressure-retaining and load-bearing equipment that operates under medium internal pressure and moderate to lower temperature conditions. Owing to their high tensile strength, stable yield performance, and reliable low-temperature toughness, SA612 plates are suitable for both static and cyclic pressure service.

 

SA612 steel plates are widely applied in the fabrication of welded pressure vessels, reactors, and pressure shells, particularly in petrochemical and chemical plants. The material's minimum yield strength of 345 MPa and tensile strength up to 725 MPa allow vessels to safely withstand internal pressure while maintaining structural integrity. Normalized delivery improves notch toughness, reducing the risk of brittle fracture during start-up, shutdown, and low-temperature operation.

 

In shell-and-tube heat exchangers and pressure-retaining shells, SA612 steel provides a balanced combination of strength and ductility, enabling it to resist thermal stress, pressure fluctuations, and welding-induced residual stress. The controlled carbon and microalloy content ensures good weldability and reliable performance of welded joints under long-term service.

 

SA612 steel plates are commonly used in spherical storage tanks for pressurized gases and liquids such as LPG, ammonia, and industrial process media. The steel's uniform mechanical properties and good impact toughness at –40℃ enhance safety margins in low-temperature environments and during seasonal temperature variations.

 

For boilers, drums, and auxiliary pressure components, SA612 steel plates provide sufficient strength for pressure containment while maintaining acceptable formability for rolling and forming operations. The material exhibits low sensitivity to bending, rolling, and deformation, making it suitable for complex vessel geometries.

 

In petrochemical and chemical processing units, SA612 steel plates are used for reactors, separators, absorbers, and pressure pipelines where stable performance under pressure, heat, and corrosive media is required. Compliance with ASME SA612/SA612M and ASTM A612/A612M standards ensures compatibility with international pressure vessel design codes.

 

SA612 steel plates are applied in power generation equipment, including pressure vessels, heat recovery systems, and auxiliary pressure components in thermal and nuclear power plants. The material's consistent quality, controlled grain size (>= ASTM No.5), and optional ultrasonic testing contribute to long-term operational reliability.

 

Nuclear-Related Pressure-Retaining Structures

For nuclear-related pressure shells and containment structures, SA612 steel plates are selected for their strict chemical control, normalized microstructure, and verified impact toughness. These characteristics are essential for ensuring safety and structural stability in critical energy infrastructure.

 

 

Compared with conventional pressure vessel steels, SA612 offers:

Improved low-temperature toughness due to normalization and microalloying

Good weldability under ASME-qualified welding procedures

These advantages make SA612 a cost-effective and technically reliable solution for modern pressure vessel fabrication.

 

 

info-536-393

 

1. What is SA612 steel plate?

SA612 steel plate is a killed carbon–manganese–silicon (C–Mn–Si) pressure vessel steel produced in accordance with ASME SA612/SA612M and ASTM A612/A612M standards.
It is designed for welded pressure vessels operating at moderate and lower temperatures, requiring high strength and reliable toughness.

 

2. What is the typical application temperature range of SA612?

SA612 steel plate is suitable for moderate and low-temperature service, and impact testing is commonly performed at –40℃.
This makes SA612 appropriate for pressure vessels exposed to:

Start-up and shutdown thermal cycling

Medium-pressure, non-cryogenic environments

 

3. What is the thickness range of SA612 steel plate?

According to ASTM A612/A612M and ASME SA612/SA612M:

Standard maximum thickness: <= 25 mm (1 inch)

In industrial production, SA612 plates may be supplied in:

Thickness range: 8 – 120 mm (subject to technical agreement)

 

P265GH+410,S355JR+410,A516Gr70+316,
A537CL1+304L,Q235B+304L,Q345B+304,
A516Gr70(NACE)+410,A537CL1+904L,
A537CL1+316L,A516Gr70+304L,A537CL1+304
,A516Gr70+410,A516Gr70+904L
2-300mm(Based plate),1-50mm(Composited plate) / UT, AR, TMCP.Normalized, Quenched and Tempered,Z Direction Test, Charpy V-Notch impact TestThe Third Party Test , Coated or Shot Blasting and Painting.
Q345A, Q345B, Q345C, Q345D, Q345E, Q390, Q420, Q460C, ST52-3, S355J2+N, SS400, SA302GrC, S275NL, 35CrMo 6 - 350 5788.56 Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection
Q245R, Q345R, Q370R, 16MnDR, 09MnNiDR, 15CrMoR, 14Cr1MoR, 12Cr2Mo1R, SA516Gr60, SA516Gr70, SA516Gr485, SA285, SA387Gr11, SA387Gr12, SA387Gr22, P265,P295,P355GH,Q245R(R-HIC),Q345R(R-HIC) 3 - 300 8650 Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection
High-Strength Plate WH785D/E,Q960D/E, Q890D/E,WH60D/E,WH70B,Q550D,Q590D,Q690D/E 8 - 120 3086.352
Wear-Resistant Plate NM360, NM400, NM450, NM500 6 - 150 3866.297
Q235qC, Q345qC, Q370qC, Q420qC, Q345qDNH, Q370qDNH, A709 - 50F - 2, A709 - 50T - 2 8 - 200 2853.621 Hot rolling, normalized ,hot rolling controlled rolling, quenched and tempered + toughness and brittleness